Thermoplastic polyurethane elastomer(PU-TPE) and energetic thermoplastic polyurethane Elastomer(E-PU-TPE) were prepared from Hexamethylene diisocyanate(HDI), 1,4-BD/AA ester polyol and glycidyl azide polymer(GAP- 2400) as an energetic material by the addition polymerization. The PU-TPE and E-PU-TPE were characterized by FT-IR and GPC. Viscometer, DSC and UTM were used to investigate the viscose behavior with a various solvent, thermal properties and mechanical properties of PU-TPE and E-PU-TPE, which are of potential interest for the development of high performance binder of energetic solid propellants.
It was found that Mw of PU-TPE and E-PU-TPEs are over 100,000 and decreased with increase of GAP-2400 contents. Tm and ΔH as thermal properties decreased and also tensile strength and elongation at break as mechanical properties decreased with increase of GAP-2400 contents.